| NEE | Testitem | Eenheid | Prestatie | Testresultaat | Testmethode | ||
| Materiaal achterkant | |||||||
| 1 | Treksterkte | MPa | ≥17 | 19.47 | ASTM D638 | ||
| 2 | Verlenging | % | ≥400 | 626 | ASTM D638 | ||
| 3 | Vicat verwekingspunt | ºC | ≥90 | 92 | ASTM D1525 | ||
| 4 | Broosheid Temperatuur | ºC | <-65 | <-65 | ASTM D2671C | ||
| 5 | Diëlektrische sterkte | MV/m | ≥25 | 33.13 | ASTM D149 | ||
| 6 | Volumeweerstand | Ω.M | ≥1*1013 | 1,1*1013 | ASTM D257 | ||
| 7 | Milieu-stressscheur | H | ≥1000 | >1000 | GB/T1842 | ||
| 8 |
Chemisch weerstand (7d) |
10% HCI |
Treksterkte | MPa | ≥85 | 104,9 | ASTM D638 |
| Verlenging | % | ≥85 | 96,3 | ASTM D638 | |||
| 10% Naa |
Treksterkte | MPa | ≥85 | 102.1 | ASTM D638 | ||
| Verlenging | % | ≥85 | 95,6 | ASTM D638 | |||
| 10% NaCl |
Treksterkte | MPa | ≥85 | 108,3 | ASTM D638 | ||
| Verlenging | % | ≥85 | 94,1 | ASTM D638 | |||
| 9 | Thermische veroudering (150ºC,168u) |
Treksterkte | MPa | ≥14 | 20.7 | ASTM D638 | |
| Verlenging | % | ≥300 | 630 | ASTM D638 | |||
| NEE. | Testitem | Eenheid | Prestatie | Tekstresultaat | Tekstmethode | |
| Kleefmiddel | ||||||
| 1 | Verzachtingspunt | ºC | ≥90 | 90,1 | ASTM E28 | |
| 2 | Broosheid Temperatuur | ºC | <-15 | <-15 | ASTM D2671C | |
| 3 | Lap-schaar | MPa | ≥1,0 | 1.5 | ASTM D1002 | |
| 4 |
Schilsterkte (23 ±2ºC) |
Staal | N/cm | ≥70 | 145,6 | ASTM D1000 |
| Primer | N/cm | ≥70 | 205,9 | ASTM D1000 | ||
| PE-laag | N/cm | ≥70 | 190,0 | ASTM D1000 | ||
| Niet-oplosmiddel epoxyprimer | ||||||
| 5 | Afschuiving van uitgeharde primer | MPa | ≥5,0 | 12 | SY/T0041 | |